Galvanic corrosion is an electrochemical process where one metal corrodes preferentially when in electrical contact with another in the presence of an electrolyte. This occurs because the dissimilar metals create a bimetallic couple, with the less noble (more active) metal acting as the anode and corroding, while the more noble metal acts as the cathode.
Galvanic Corrosion
- Luigi Galvani
- Alessandro Volta
The driving force for galvanic corrosion is the difference in electrode potential between the two dissimilar metals. When connected, they form a short-circuited electrochemical cell. The metal with the more negative electrode potential (the less noble metal) becomes the anode and undergoes oxidation, releasing electrons and metal ions into the electrolyte. For example, when zinc is in contact with steel in seawater, zinc oxidizes: \(Zn \\rightarrow Zn^{2+} + 2e^-\).
Simultaneously, the more noble metal (with the more positive potential) becomes the cathode, where a reduction reaction occurs. The electrons released by the anode travel through the metallic connection to the cathode. In a neutral or acidic electrolyte like seawater, the reduction reaction is typically the reduction of oxygen: \(O_2 + 2H_2O + 4e^- \\rightarrow 4OH^-\).
The rate of galvanic corrosion is influenced by several factors, including the potential difference between the metals (a larger difference leads to faster corrosion), the ratio of the cathode-to-anode surface area (a large cathode and small anode is the worst-case scenario, leading to rapid localized corrosion of the anode), and the conductivity of the electrolyte. The Galvanic Series, which ranks metals and alloys by their electrochemical potential in a specific electrolyte (commonly seawater), is a critical tool for engineers to predict and prevent this type of corrosion by selecting compatible materials.
Type
Disruption
Usage
Precursors
- Luigi Galvani’s discovery of ‘animal electricity’ (1780s)
- Alessandro Volta’s invention of the voltaic pile (1800)
- Michael Faraday’s laws of electrolysis (1834)
Applications
- sacrificial anodes for protecting ship hulls and pipelines
- galvanized steel (zinc coating on steel)
- batteries (the fundamental principle)
- understanding material compatibility in engineering design
Patents:
Potential Innovations Ideas
Professionals (100% free) Membership Required
You must be a Professionals (100% free) member to access this content.
AVAILABLE FOR NEW CHALLENGES
Mechanical Engineer, Project or R&D Manager
Available for a new challenge on short notice.
Contact me on LinkedIn
Plastic metal electronics integration, Design-to-cost, GMP, Ergonomics, Medium to high-volume devices & consumables, Regulated industries, CE & FDA, CAD, Solidworks, Lean Sigma Black Belt, medical ISO 13485
We are looking for a new sponsor
Your company or institution is into technique, science or research ?
> send us a message <
Receive all new articles
Free, no spam, email not distributed nor resold
or you can get your full membership -for free- to access all restricted content >here<
Historical Context
Galvanic Corrosion
(if date is unknown or not relevant, e.g. "fluid mechanics", a rounded estimation of its notable emergence is provided)
Related Invention, Innovation & Technical Principles