Maison » Corrosion par piqûres

Corrosion par piqûres

1930
Échantillon de métal présentant une corrosion par piqûres dans un laboratoire de science des matériaux.

(generate image for illustration only)

Pitting corrosion is a localized form of corrosion that leads to the creation of small holes, or ‘pits,’ in a metal. It is one of the most destructive forms because it is difficult to detect, predict, and design against. Pitting can cause catastrophic failure of a structure with only a small percentage of total mass loss.

Pitting is an autocatalytic process. It typically initiates at small surface defects, inclusions, or scratches, especially on passive metals like stainless steel or aluminum. The process begins with the local breakdown of the passive film, often triggered by aggressive anions, most notably chloride ([latex]Cl^-[/latex]). Once the film is breached, an active corrosion cell is established. The small area of exposed metal becomes the anode, and the large surrounding passive surface becomes the cathode.

Inside the pit, metal dissolution occurs, for example [latex]Fe \\rightarrow Fe^{2+} + 2e^-[/latex]. The resulting positive metal ions attract negative chloride ions from the solution into the pit to maintain charge neutrality. This leads to the formation of metal chlorides, such as [latex]FeCl_2[/latex], which then hydrolyze with water: [latex]FeCl_2 + 2H_2O \\rightarrow Fe(OH)_2 + 2HCl[/latex]. This reaction produces hydrochloric acid, which dramatically lowers the pH inside the pit, making the local environment highly acidic and aggressive. This increased acidity further accelerates metal dissolution and prevents the passive film from reforming, creating a self-sustaining cycle that causes the pit to grow deeper. The exterior surface remains protected, masking the severe damage occurring beneath.

UNESCO Nomenclature: 3314
- Science des matériaux

Taper

Processus chimique

Perturbation

Substantiel

Usage

Utilisation généralisée

Précurseurs

  • Discovery and use of passive metals like stainless steel
  • Understanding of electrochemical cells and passivation
  • Increased use of materials in chloride-rich environments (e.g., marine, chemical industry)

Applications

  • failure analysis in chemical processing plants
  • inspection protocols for pipelines and storage tanks
  • materials selection for marine environments
  • design of medical implants to avoid in-vivo pitting

Brevets:

NA

Idées d'innovations potentielles

!niveaux !!! Adhésion obligatoire

Vous devez être membre de l'association pour accéder à ce contenu.

S’inscrire maintenant

Vous êtes déjà membre ? Connectez-vous ici
Related to: pitting corrosion, localized corrosion, passive film, chloride, stainless steel, autocatalytic, failure analysis, corrosion pit.

Laisser un commentaire

Votre adresse e-mail ne sera pas publiée. Les champs obligatoires sont indiqués avec *

DISPONIBLE POUR DE NOUVEAUX DÉFIS
Ingénieur mécanique, chef de projet, ingénierie des procédés ou R&D
Développement de produits efficace

Disponible pour un nouveau défi dans un court délai.
Contactez-moi sur LinkedIn
Intégration électronique métal-plastique, Conception à coût réduit, BPF, Ergonomie, Appareils et consommables de volume moyen à élevé, Production allégée, Secteurs réglementés, CE et FDA, CAO, Solidworks, Lean Sigma Black Belt, ISO 13485 médical

Nous recherchons un nouveau sponsor

 

Votre entreprise ou institution est dans le domaine de la technique, de la science ou de la recherche ?
> envoyez-nous un message <

Recevez tous les nouveaux articles
Gratuit, pas de spam, email non distribué ni revendu

ou vous pouvez obtenir votre adhésion complète - gratuitement - pour accéder à tout le contenu restreint >ici<

Contexte historique

(si la date est inconnue ou non pertinente, par exemple « mécanique des fluides », une estimation arrondie de son émergence notable est fournie)

Inventions, innovations et principes techniques connexes

Retour en haut

Vous aimerez peut-être aussi