Corrosión por picaduras

1930
Muestra de metal que presenta corrosión por picadura en un laboratorio de ciencia de los materiales.

(generate image for illustration only)

Pitting corrosion is a localized form of corrosion that leads to the creation of small holes, or ‘pits,’ in a metal. It is one of the most destructive forms because it is difficult to detect, predict, and design against. Pitting can cause catastrophic failure of a structure with only a small percentage of total mass loss.

Pitting is an autocatalytic process. It typically initiates at small surface defects, inclusions, or scratches, especially on passive metals like stainless steel or aluminum. The process begins with the local breakdown of the passive film, often triggered by aggressive anions, most notably chloride ([latex]Cl^-[/latex]). Once the film is breached, an active corrosion cell is established. The small area of exposed metal becomes the anode, and the large surrounding passive surface becomes the cathode.

Inside the pit, metal dissolution occurs, for example [latex]Fe \\rightarrow Fe^{2+} + 2e^-[/latex]. The resulting positive metal ions attract negative chloride ions from the solution into the pit to maintain charge neutrality. This leads to the formation of metal chlorides, such as [latex]FeCl_2[/latex], which then hydrolyze with water: [latex]FeCl_2 + 2H_2O \\rightarrow Fe(OH)_2 + 2HCl[/latex]. This reaction produces hydrochloric acid, which dramatically lowers the pH inside the pit, making the local environment highly acidic and aggressive. This increased acidity further accelerates metal dissolution and prevents the passive film from reforming, creating a self-sustaining cycle that causes the pit to grow deeper. The exterior surface remains protected, masking the severe damage occurring beneath.

UNESCO Nomenclature: 3314
- Ciencia de los materiales

Tipo

Proceso químico

Disrupción

Sustancial

Utilización

Uso generalizado

Precursores

  • Discovery and use of passive metals like stainless steel
  • Understanding of electrochemical cells and pasivación
  • Increased use of materials in chloride-rich environments (e.g., marine, chemical industry)

Aplicaciones

  • failure analysis in chemical processing plants
  • inspection protocols for pipelines and storage tanks
  • materials selection for marine environments
  • design of medical implants to avoid in-vivo pitting

Patentes:

NA

Posibles ideas innovadoras

Membresía obligatoria de Professionals (100% free)

Debes ser miembro de Professionals (100% free) para acceder a este contenido.

Únete ahora

¿Ya eres miembro? Accede aquí
Related to: pitting corrosion, localized corrosion, passive film, chloride, stainless steel, autocatalytic, failure analysis, corrosion pit.

Deja una respuesta

Tu dirección de correo electrónico no será publicada. Los campos obligatorios están marcados con *

DISPONIBLE PARA NUEVOS RETOS
Ingeniero Mecánico, Gerente de Proyectos, Ingeniería de Procesos o I+D
Desarrollo eficaz de productos

Disponible para un nuevo desafío a corto plazo.
Contáctame en LinkedIn
Integración de electrónica de metal y plástico, diseño a coste, GMP, ergonomía, dispositivos y consumibles de volumen medio a alto, fabricación eficiente, industrias reguladas, CE y FDA, CAD, Solidworks, cinturón negro Lean Sigma, ISO 13485 médico

Estamos buscando un nuevo patrocinador

 

¿Su empresa o institución se dedica a la técnica, la ciencia o la investigación?
> Envíanos un mensaje <

Recibe todos los artículos nuevos
Gratuito, sin spam, correo electrónico no distribuido ni revendido.

o puedes obtener tu membresía completa -gratis- para acceder a todo el contenido restringido >aquí<

Contexto histórico

(si se desconoce la fecha o no es relevante, por ejemplo "mecánica de fluidos", se ofrece una estimación redondeada de su notable aparición)

Invención, innovación y principios técnicos relacionados

Scroll al inicio

También te puede interesar