Galvanic corrosion is an electrochemical process where one metal corrodes preferentially when in electrical contact with another in the presence of an electrolyte. This occurs because the dissimilar metals create a bimetallic couple, with the less noble (more active) metal acting as the anode and corroding, while the more noble metal acts as the cathode.

The driving force for galvanic corrosion is the difference in electrode potential between the two dissimilar metals. When connected, they form a short-circuited electrochemical cell. The metal with the more negative electrode potential (the less noble metal) becomes the anode and undergoes oxidation, releasing electrons and metal ions into the electrolyte. For example, when zinc is in contact with steel in seawater, zinc oxidizes: [latex]Zn \\rightarrow Zn^{2+} + 2e^-[/latex].

Simultaneously, the more noble metal (with the more positive potential) becomes the cathode, where a reduction reaction occurs. The electrons released by the anode travel through the metallic connection to the cathode. In a neutral or acidic electrolyte like seawater, the reduction reaction is typically the reduction of oxygen: [latex]O_2 + 2H_2O + 4e^- \\rightarrow 4OH^-[/latex].

The rate of galvanic corrosion is influenced by several factors, including the potential difference between the metals (a larger difference leads to faster corrosion), the ratio of the cathode-to-anode surface area (a large cathode and small anode is the worst-case scenario, leading to rapid localized corrosion of the anode), and the conductivity of the electrolyte. The Galvanic Series, which ranks metals and alloys by their electrochemical potential in a specific electrolyte (commonly seawater), is a critical tool for engineers to predict and prevent this type of corrosion by selecting compatible materials.

UNESCO Nomenclature: 2203
– Electrochemistry

类型

Chemical Process

Disruption

Foundational

使用方法

Widespread Use

Precursors

  • Luigi Galvani’s discovery of ‘animal electricity’ (1780s)
  • Alessandro Volta’s invention of the voltaic pile (1800)
  • Michael Faraday’s laws of electrolysis (1834)

应用

  • sacrificial anodes for protecting ship hulls and pipelines
  • galvanized steel (zinc 涂层 on steel)
  • batteries (the fundamental principle)
  • understanding material compatibility in engineering design

专利:

Potential Innovations Ideas

级别需要会员

您必须是!!等级!!会员才能访问此内容。

立即加入

已经是会员? 在此登录
Related to: galvanic corrosion, bimetallic couple, electrochemistry, anode, cathode, electrolyte, galvanic series, sacrificial anode

发表回复

您的邮箱地址不会被公开。 必填项已用 * 标注

迎接新挑战
机械工程师、项目或研发经理
有效的产品开发

可在短时间内接受新的挑战。
通过 LinkedIn 联系我
塑料金属电子集成、成本设计、GMP、人体工程学、中高容量设备和耗材、受监管行业、CE 和 FDA、CAD、Solidworks、精益西格玛黑带、医疗 ISO 13485

我们正在寻找新的赞助商

 

您的公司或机构从事技术、科学或研究吗?
> 给我们发送消息 <

接收所有新文章
免费,无垃圾邮件,电子邮件不分发也不转售

或者您可以免费获得完整会员资格以访问所有受限制的内容>这里<

(if date is unknown or not relevant, e.g. "fluid mechanics", a rounded estimation of its notable emergence is provided)

Related Invention, Innovation & Technical Principles

滚动至顶部

你可能还喜欢